TECHNET Archives

June 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Thu, 5 Jun 2008 06:48:22 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Chandler <[log in to unmask]>
Subject:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="ISO-8859-1"
From:
Brian Chandler <[log in to unmask]>
Parts/Attachments:
text/plain (26 lines)
Linda,

If you are talking about compliant pins, most can be pressed out. Is it a
header or an integrated housing? The difficult thing is the ability to
support the PCB while you press the pins out. A slow press rate is
recommended (12mm/min).

Consulting the supplier is still a good idea since some pins are so
aggressive, they will damage the PCB when removed. Also, the length of time
the connector has been in the board can be an issue due to "cold welding".

If you have displacement pins, I agree with others that repair should not be
attempted.

Brian

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2