TECHNET Archives

June 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 10 Jun 2008 20:24:14 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Subject:
MIME-Version:
1.0
content-transfer-encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Joyce Koo <[log in to unmask]>
Parts/Attachments:
text/plain (154 lines)
Let. All use polyimade.  Cheaper than feed politicians.
--------------------------
Sent using BlackBerry


----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Tue Jun 10 15:52:35 2008
Subject: Re: [TN] Flame retardants ignite controversy - Posted without comment

OK so the EU through Oko is recommending banning them why?. 

Should they not just enforce the Basel convention or is this just too
simplistic a view. Seems that Oko  are trying to band aid the Basel
convention rather than address the issue and recommend enforcement??

One thing I can pretty much guarantee is that the eventual replacements for
flame retardents and the laminate in which they reside will not result in
the lemming like leap that occurred with lead free finishes by the component
manufacturers.

The reason I put forward for this is that the laminate industry already
provides a plethora of laminate types. So adding another range will not make
much difference particularly when they are more expensive and device
manufacturers actually do run 2 product codes down their lines one compliant
and expensive and one non compliant and aimed at the rest of the World
outside the EU ( Yes "EU politically correct land" there is a World out
there - it just tends to put more thought into these issues though)
 
Just my thoughts
 
John Burke
 
(408) 515 4992

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joe Fjelstad
Sent: Tuesday, June 10, 2008 12:22 PM
To: [log in to unmask]
Subject: [TN] Flame retardants ignite controversy - Posted without comment

 
for your  consideration...
Joe
http://www.edn.com/blog/570000257/post/1740027974.html?nid=3357&rid=20860561
3
Tuesday, June 10, 2008
 
Flame retardants ignite  controversy
 
Jun 10 2008 7:31AM 
Accurate figures are difficult to obtain, but it has been estimated that  
fires kill around 10,000 people a year globally, in which the cause is  
attributed to faulty electrical wiring in buildings and in electrical
equipment.  Flame 
retardants have been used very effectively in a wide variety of electrical  
equipment to prevent fires, reduce their seriousness and also to delay onset
to 
 allow people more time to evacuate. In fact, research has shown that when 
flame  retardants are used as additives to plastics, the amount of time to 
escape is  increased by 15 times. Since they were introduced, thousands of
lives 
have been  saved, and so there is no doubt about their value. 
Many types of plastics burn very easily. It has been estimated that the  
plastics in a typical TV set are equivalent to 1.5 gallons of gas, not
something  
consumers want in their living rooms!  However, only around 12% of plastics

contain flame retardants. Some types are inherently resistant to fire, such
as  
rigid PVC, and so do not need flame retardant additives. Some equipment is 
not  at risk such as battery powered products like mobile phones because of
the 
low  voltages used, and therefore flame retarded plastics are not needed. 
Mobile  phone battery chargers, however, do need to have flame retardants as
they 
are  powered at standard voltages, and so arcing and high temperatures can 
occur if  there is a defect. 
But BFRs (brominated flame retardants) are now at the center of considerable

debate. The review of the ROHS directive, undertaken by the German 
organization  Oko on behalf of the European Commission, is looking at a
significant 
number of  them, along with 46 other chemical compounds, and may well
recommend 
the  restriction of some, or all of them. 
So, why will they be banned when many have already been tested, and it was  
concluded that they pose no threat to human health and the environment? 
Well, Oko is recommending a ban on all organobromine and organochlorine  
compounds, including brominated flame retardants because of "backyard
recycling"  
of WEEE (Waste Electrical and Electronic Equipment) in countries that do not

have the know-how, or facilities, to dismantle safely. 
The toxic fumes created by backyard and roadside fires are having a  
significant affect on human health, even causing death. 
While the Basel Convention should stop the shipping of WEEE to such  
countries, a lot of the scrap still comes from the likes of the United
States,  which 
has not yet ratified it. 
Flame retardants seem a classic example of a need for a risk-benefit balance

based on assessments that the ROHS directive and REACH regulations were 
designed  to resolve. It's a trade-off between safe furniture, fabrics, and 
electronics or  the fatalities caused in the poorer villages of China,
India, and 
Africa. 






**************Vote for your city's best dining and nightlife. City's Best 
2008.      (http://citysbest.aol.com?ncid=aolacg00050000000102)

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2