Dear technetters,
Is anybody using SN100 (or other high Sn alloys) for SMT reflow soldering applications? what have your experiences been with this alloy?
I have a PCB with a BGA, that is cracking due to mechanical stress (that is not SMT process related), we have a combination of solder cracking, and pad cratering. The PCB currently uses SAC305. We also build a SnPb variant of the same exact board with no issues (the bare board material is different for SnPb and LF versions). I was therefore wondering whether SCA305 alloy properties could be a contributing factor this defect. How does the ductility and shear strength of SN100C compare to SAC305 and 67-37SNPb alloy?
Regards,
Amol
WARNING: Export Control
This document may contain technical data within the definition of the
International Traffic in Arms Regulations (ITAR), and subject to the Export
Control Laws of the U.S. Government. Transfer of such data by any means to a
foreign person, whether in the United States or abroad, without proper export
authorization or other approval from the U.S. Department of State is
prohibited.
CONFIDENTIALITY NOTICE:
This e-mail, and any attachments, is for the sole use of the intended
recipient(s) and may contain information that is confidential and
protected from disclosure under the law. Any unauthorized review, use,
disclosure, or distribution is prohibited. If you are not the intended
recipient, please contact the sender by reply e-mail, and delete/destroy
all copies of the original message and attachments.
Thank you.
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|
|
|