Ni Hao ?????
the other lab...is recommending using data logger (not Event detector) -->, 300 ohms, 10 events (maximum), 1 msec (not typo error) duration
(maximum), report first verified as time-to-failure
I am going for solder joint....fine pitch QFN and LGA, high pins count BGA, etc.
________________________________
From: TechNet on behalf of Werner Engelmaier /*
Sent: Fri 6/27/2008 7:56 PM
To: [log in to unmask]
Subject: Re: [TN] IPC 9701- table 4.4- failure definition
Ni hao GA Tan,
The preferred failure definitiion is
a) Event detector, 1000 ohms, 10 events (maximum), 1 micro-second duration
(maximum), report first verified as time-to-failure.
It is better yet to use:
Event detector, 300 ohms, 10 events (maximum), 1 micro-second duration
(maximum), report first verified as time-to-failure [I take it 1msec is a typo].
b) gives you somewhat later failure indication, depending on what it is you
are testing.
It is considered a failure with 5 scans more than 20% resistance increase
over the initial nominal resisistance at the same temperature.
Regards,
Werner Engelmaier
?????
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com
**************
Gas
prices getting you down? Search AOL Autos for fuel-efficient used cars.
(http://autos.aol.com/used?ncid=aolaut00050000000007)
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|