TECHNET Archives

June 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Mon, 23 Jun 2008 08:26:25 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (59 lines)
Yes, too little P will allow the acidity of the gold bath to pit the
nickle surface. I think pitting is a better word. And I agree with
Werner's definition. 
So what is the definition of Brittle Intermetallic Failure as opposed to
Black Pad? Or did I miss that?

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier /*
Sent: Friday, June 20, 2008 3:05 AM
To: [log in to unmask]
Subject: Re: [TN] [LF] [TN] SN100 for Reflow Application

Hi Vladimir,
For BP I am really only concerned about the surface, so EDS is
fine--after all it is the interface surface that is weak. 
Cavitation (as a ME that word bothers me because cavitation is what a
propeller does in water) is a sign of the P notdoing its job.
So I stand by my definition.



Werner Engelmaier
Future workshops:
Solder Joint Reliability: Parts 1 through 4, July 17/18, Thal,
Switzerland Pb-Free Soldering Processes-Survival, Quality, Reliability,
August 18, Orlando Reliability Issues with Lead-Free Soldering
Processes, September 22, Schaumburg Failure Mode and Root Cause Analyses
Reliability (Fatigue, Brittle Fracture, ENIG), September 22, Schaumburg



**************
Gas prices getting you down? Search AOL Autos for fuel-efficient used
cars.
      (http://autos.aol.com/used?ncid=aolaut00050000000007)

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2