TECHNET Archives

June 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 18 Jun 2008 12:50:44 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Kane, Amol (349)" <[log in to unmask]>
Subject:
From:
"Kane, Amol (349)" <[log in to unmask]>
Content-Transfer-Encoding:
base64
In-Reply-To:
Content-Type:
text/plain; charset="utf-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (1 lines)
Dear Valdimir,

Can you please clarify your E-mail below? Do you think I may be dealing with black pad?



Regards,

From: Igoshev, Vladimir [mailto:[log in to unmask]]

Sent: Wednesday, June 18, 2008 10:55 AM

To: [log in to unmask]; Kane, Amol (349)

Subject: Re: [LF] [TN] SN100 for Reflow Application





Hi Amol,



The thickness of intermetallic layer does not indicate whether you might deal with BP or not, but the fact that you got laminate cracks does.



Regards,



Vladimiir



----- Original Message -----

From: Leadfree <[log in to unmask]>

To: [log in to unmask] <[log in to unmask]>

Sent: Wed Jun 18 10:33:12 2008

Subject: Re: [LF] [TN] SN100 for Reflow Application



Hi Pete,

We will not be using the DICY cured laminate in a LF process. It wont withstand LF process temperatures. yes, we did observe a P rich area and a rough Ni surface. However, a presence of a thick intermetallic layer rules out black pad. it does reflect a plating bath that Is potentially unbalanced wrt the chemical composition. However, the SnPb version of the board is also ENIG and from the same board supplier. Therefore all things being equal (plating wise), we see cracks only with the LF assembly.



All the obvious SMT process steps (Solder deposition, solder ht, reflow temps etc.,) were checked to ensure accuracy.



Regards,

Amol





-----Original Message-----

From: Pete Houwen [mailto:[log in to unmask]]

Sent: Wednesday, June 18, 2008 9:53 AM

To: [log in to unmask]; Kane, Amol (349)

Subject: Re: [TN] SN100 for Reflow Application



Amol,



If you are joints that much more prone to failure, don't rule out your process

just because they aren't failing during the process.



Are these ENiG plated boards?  When you did your cross sections, did you do

any analysis of the interfacial?  Are you getting P-enriched zones?  Are there

voids - large or micro, in the joints or balls?  Are the soldermask openings and

registration the same on both versions?  Do you inspect the paste deposition

to make sure the stencil is releasing the lead free solder as it did with tin/lead?



While the fractures aren't showing up until you apply mechanical stress, the

process itself could be weakening the joints, and that doesn't always show up

on all of the balls, or even the same ones consistently.  Though pad cratering

indicates that at least at those pads, the joint was stronger than the laminate.



Be careful using dicy cured epoxies with lead free process temperatures.  A

whole 'nother can o' worms.



Pete









WARNING:  Export Control

This document may contain technical data within the definition of the

International Traffic in Arms Regulations (ITAR), and subject to the Export

Control Laws of the U.S. Government.  Transfer of such data by any means to a

foreign person, whether in the United States or abroad, without proper export

authorization or other approval from the U.S. Department of State is

prohibited.



CONFIDENTIALITY NOTICE:

This e-mail, and any attachments, is for the sole use of the intended

recipient(s) and may contain information that is confidential and

protected from disclosure under the law. Any unauthorized review, use,

disclosure, or distribution is prohibited. If you are not the intended

recipient, please contact the sender by reply e-mail, and delete/destroy

all copies of the original message and attachments.

Thank you.



-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Leadfree

To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)

Search previous postings at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-------------------------------------------------------------------------------







WARNING:  Export Control 

This document may contain technical data within the definition of the 

International Traffic in Arms Regulations (ITAR), and subject to the Export 

Control Laws of the U.S. Government.  Transfer of such data by any means to a 

foreign person, whether in the United States or abroad, without proper export 

authorization or other approval from the U.S. Department of State is 

prohibited. 

 

CONFIDENTIALITY NOTICE: 

This e-mail, and any attachments, is for the sole use of the intended 

recipient(s) and may contain information that is confidential and 

protected from disclosure under the law. Any unauthorized review, use, 

disclosure, or distribution is prohibited. If you are not the intended 

recipient, please contact the sender by reply e-mail, and delete/destroy 

all copies of the original message and attachments. 

Thank you.

ATOM RSS1 RSS2