Ingemar,
Good afternoon!
Depending upon the robustness of the solder fillet, I can visualize a
problem with the circumference of the pad/s lifting/peeling during temp
cycles. Large, heavy, robust solder fillets leading to eventual open or
intermittent circuits. Whereas light, delicate, thin fillets survive
nicely.
In my minds-eye, I picture the perimeter as being a relatively high
stress area and not an exceptionally good place to put an interconnect
via - keep it in the center/neutral stress point. Adding a protuberance
to the perimeter would seem like adding insult to injury.
Back in the olden days of conventional thick films, we would actually
put down a ring of dielectric around the edge of a circular pad such as
this to 'help hold it down'. Assuming the solderable conductor is
co-fired in your case, that would seemingly be of negligible benefit.
You are being a little tight-lipped about the problem observed, but I
bet that you are seeing pad lifting at the edges.
.... drum roll ......
.... and the answer is _________
Have a good day!
:-) Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
Sent: Thursday, May 29, 2008 5:59 AM
To: [log in to unmask]
Subject: [TN] via placement in LTCC
Mr Trikeman or someone else with one foot in LTCC, need advice.
Imagine a 90 degree SMA coax connector for solder mounting on LTCC
silver thickfilm pads.
The RF connector center pin is soldered to a circular thickfilm pad,
that is double the diameter of the RF connector center pin.
Now, these pads communicate by means of vias in the blue tape (the
dielectric). First, the vias were placed in the center of the circular
thickfilm pad, later, someone decided to move the via to the periphery,
i.e. off center. The designer has added a small land (ear)to the
circular thickfilm pad, and it's here the vias are removed.
The later design has caused some trouble. Seems as the off-center via
placement wasn't good.
I got some ideas what it's all about, but first I would like to hear
with you, guys
Hope my description is understandable.
Inge
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
THE INFORMATION CONTAINED IN THIS E-MAIL MESSAGE AND ANY ATTACHMENTS SENT FROM GENTEX CORPORATION IS GENTEX CONFIDENTIAL INFORMATION INTENDED ONLY FOR THE PERSONAL USE OF THE INDIVIDUAL OR ENTITY NAMED ABOVE. If you are not the intended recipient, you are hereby notified that any review, distribution, or copying of this communication is strictly prohibited. If you have received this communication in error, please immediately notify the sender by return e-mail, and delete this e-mail message and any attachments from your computer. [gntx v.1]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|