Usually reduced ID is more relevant with HASL boards because its higher
thickness and less control on thickness.
Do a cross section I suppose you will find the reason
Ido Mashall
Fax: +972-4-6376666, Tel: +972-77-2127172,
www.beyond-materials.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Croslin, Robert
Sent: Tuesday, May 27, 2008 4:57 PM
To: [log in to unmask]
Subject: [TN] PTH's With Immersion Silver
We've been using immersion silver on our boards for quite a while with
great success, but in a recent run of a new product, we had the boards
come in with the PTH's used to mount RCA and audio connectors smaller
that usual. The parts came in on the large end so it became very
difficult for the operator to insert them into the board. Both holes
and parts were in tolerance and the holes were specified at the
recommended diameters. Our CM has a woman who spent 20 years working in
pcb fab houses and she tells me that it's not at all unusual to have IS
boards with reduced ID's on the holes as opposed to HASL. Has anyone
else experienced this? If this is the case, we'll have to adjust for
this in the future, but it would be useful to know if this was an
anomaly or a normal condition?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
--
No virus found in this incoming message.
Checked by AVG.
Version: 7.5.524 / Virus Database: 269.24.1/1468 - Release Date: 26/05/2008
15:23
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|