TECHNET Archives

May 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Phil Nutting <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Phil Nutting <[log in to unmask]>
Date:
Tue, 27 May 2008 08:57:03 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (118 lines)
Ah, new information.

Thanks Rudy, Brian and Doug.

For our boards with the slip ring dust it looks like a quick 1 minute wash will remove the dust without attacking the conformal coating.  Having said that I will do some testing to confirm this.

Phil

________________________________
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Tuesday, May 27, 2008 8:51 AM
To: TechNet E-Mail Forum; Phil Nutting
Subject: Re: [TN] Conformal coating washing off


Phil,
Most of the pure acrylic coatings are not that good in terms of chemical resistance.  We do not allow our conformally coated assemblies (Humiseal 1B31) to go through saponified aqueous cleaning for just the reason you are seeing, the adhesion gets affected and the coating comes off.

Doug Pauls



Phil Nutting <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>

05/27/2008 07:46 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Phil Nutting <[log in to unmask]>




To
        [log in to unmask]
cc

Subject
        Re: [TN] Conformal coating washing off







Brian,

I guess I should add that we have been using this conformal coating for about six years with "great success".  It has only been in this test of a new washing system that we are seeing the coating peel off.  The DI wash in my original post was the wash step after soldering with an OA flux.  Maybe the detergent in the wash system is really good for cleaning conformal coating off the boards... if that was what I really wanted.

Phil

-----Original Message-----
From: Brian Ellis [mailto:[log in to unmask]]
Sent: Saturday, May 24, 2008 2:04 AM
To: TechNet E-Mail Forum; Phil Nutting
Subject: Re: [TN] Conformal coating washing off

Some types of solder mask contain nasties that may prevent a decent
adhesion of a CC or they may not have been properly polymerised, leaving
insoluble monomers or other components on the surface. I suggest you
start looking in this direction.

Brian

Phil Nutting wrote:
> We are using Chemtronics Konform AR on some circuit boards.  The boards are batch washed in DI water and pre-baked prior to coating and then cured in a 60° or 77° C oven.
>
> In a recent test of a new washing system where we are removing slip ring dust (brass and carbon) on these boards and dielectric oil from other boards and aluminum castings, I noticed the conformal coating peeling off in sheets after both the wash and DI rinse cycles.  Both wash and rinse are between 140 and 150° F.
>
> Is this stuff peeling off because of the water temperature, poor pre-coating prep or possibly something else?
>
> Thanks in advance,
>
> Phil
>
> Note: All the information contained in this e-mail and its attachments is proprietary to Kaiser Systems, Inc. and it may not be reproduced without the prior written permission of sender.  If you have received this email in error, please immediately return it to sender and delete the copy you received.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>



Note: All the information contained in this e-mail and its attachments is proprietary to Kaiser Systems, Inc. and it may not be reproduced without the prior written permission of sender.  If you have received this email in error, please immediately return it to sender and delete the copy you received.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


________________________________
Note: All the information contained in this e-mail and its attachments is proprietary to Kaiser Systems, Inc. and it may not be reproduced without the prior written permission of sender. If you have received this email in error, please immediately return it to sender and delete the copy you received.


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2