Hi Kenny
Be careful. IVF in Sweden demonstrated that prolonged exposure to
"hot" test solution (>30DegC) can induce a rise in the Resistivity or
Conductivity reading because you begin to leach out the (commonly
bromine) flame retardant out of the laminate.
Graham Naisbitt
On 22 May 2008, at 18:29, Ken Bloomquist wrote:
> Good Day All,
>
> We are having a discussion about the specific gravity of the 75%/25%
> solution in our ROSE tester. The question revolves around testing it
> hot or
> cold.
>
> Our ROSE tester runs at 112 degrees F and would like to know whether
> we
> should test the SG at hot or cold. If so what would we expect for a
> reading?
>
> Thanks all,
>
> KennyB
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following
> text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]
> : SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]
> : SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask]
> or 847-615-7100 ext.2815
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|