Visual and ionic testing by Omega meter. It was a preliminary tests more is schedule in the near future (p.s. we use it in a vapor degreaser).
We use Vertrel SMT (looks like the same as Vertrel MS-755) which does not attack plastics.
Regards,
Gil
-----Original Message-----
From: Hernefjord Ingemar [mailto:[log in to unmask]]
Sent: Thursday, May 22, 2008 9:51 AM
To: TechNet E-Mail Forum; Zilber Gil
Subject: RE: [TN] Are these substances OK for use in electronics
What tests, if I may?
/Inge
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Zilber Gil
Sent: den 22 maj 2008 10:39
To: [log in to unmask]
Subject: Re: [TN] Are these substances OK for use in electronics
Vertrel was developed by DuPont as a "Green" replacement for cleaning solvent. We performed some tests on it and received very good results (compare to Abzol), and it is also been approved by some Aerospace companies.
It as Zero ozone depletion potential
Excellent toxicity profile
Design for electronics - high material compatibility
Regards,
Dr. Gil Zilber
Technologist, Elta system Ltd.
Tel. +972-8-8577240
Mobile +972-54-4983222
http://www.iai.co.il/site/en/iai.asp?pi=17887
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Charlie Pitarys
Sent: Thursday, May 22, 2008 8:59 AM
To: [log in to unmask]
Subject: Re: [TN] Are these substances OK for use in electronics
Combined ingredients in the can togther you have a non haz/non flammable mixture. the specific msds will comfirm that. The Nitromethane is probably the propellant media.
They are safe for electronics and have been in use for many years.
Are they effective cleaners on your assemblies should be the real question. They are very much a niche cleaner and efficacy against certain no clean formulas should be tested first.
For water soluble /OA fluxes DO NOT USE !! The results will be a horrible hard white residue mess.
Plastics such as acrylics and other polycarb blends used for switch covers etc. should be avoided.
________________________________
From: TechNet on behalf of Ioan Tempea
Sent: Wed 5/21/2008 12:32 PM
To: [log in to unmask]
Subject: Re: [TN] Are these substances OK for use in electronics
Vertrel MS-755 and MS-780 from Miller Stephenson.
Thanks,
Ioan
________________________________
De : [log in to unmask] [mailto:[log in to unmask]]
Envoyé : May 21, 2008 12:26 PM
À : TechNet E-Mail Forum; Ioan Tempea
Objet : Re: [TN] Are these substances OK for use in electronics
Ioan,
What is the actual name of the product? I would expect the fluoronated materials to be global warmers and the methanol and nitromethane go boom around flame.
Doug Pauls
Ioan Tempea <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
05/21/2008 11:04 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to Ioan Tempea <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] Are these substances OK for use in electronics
Dear Technos,
I've got one for the chemists: a customer of ours requests us to clean their boards with 2 spray canned products. Here's the stuff that's inside of them:
1,1,1,2,3,4,4,5,5,5-Decafluoropentane
Trans,1,2-Dichloroethylene
Methanol
Nitromethane
1,1,1,2-Tetrafluoroethane
Are they safe for the product? What about the production personnel and the environment?
Thanks,
Ioan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
The information contained in this communication is proprietary to Israel Aerospace Industries Ltd., ELTA Systems Ltd.
and/or third parties, may contain classified or privileged information, and is intended only for the use of the intended addressee thereof. If you are not the intended addressee, please be aware that any use, disclosure, distribution and/or copying of this communication is strictly prohibited.
If you receive this communication in error, please notify the sender immediately and delete it from your computer. Thank you.
This message is processed by the PrivaWall Email Security Server.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
This message is processed by the PrivaWall Email Security Server.
The information contained in this communication is proprietary to Israel Aerospace Industries Ltd., ELTA Systems Ltd.
and/or third parties, may contain classified or privileged information, and is intended only for
the use of the intended addressee thereof. If you are not the intended addressee, please be aware
that any use, disclosure, distribution and/or copying of this communication is strictly prohibited.
If you receive this communication in error, please notify the sender immediately and delete it from
your computer. Thank you.
This message is processed by the PrivaWall Email Security Server.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|