Subject:
From:
Jack Olson <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Jack Olson <[log in to unmask]>
Date:
Tue, 20 May 2008 09:36:29 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (64 lines)
Well, since our supplier hadn't seen this condition in their microsections,
and the independent lab used different equipment (Scanning Electron
Microscope
and Differential Interference Contrast photography), the question became
whether
the supplier's lab could even see the condition if it was present.

The independent lab still has the sample panel with the known condition, and
they
agreed to send back half of the panel so the supplier can experiment with
it.
In the meantime, our company issued a corrective action request so we get
some
kind of follow-up on the results.

Thanks to everyone who looked at the evidence and sent their opinion.
http://frontdoor.biz/PCBportal/bluevoid.jpg

p.s. I think its kind of fun to do this (especially when it is not MY
company's sample)
Maybe we should have more community "case studies", I find the group
feedback to be very educational, especially when the descriptions in
IPC-A-600
are vague.

Thanks again.
onward thru the fog,
Jack

-----Original Message-----

What became of this issue?   I have not seen any more threads of e-mail.

Victor,

From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: Tuesday, April 29, 2008 9:59 PM
To: [log in to unmask]
Subject: Re: [TN] Blue Voids

Are the voids in the glass bundle or between the glass bundle and the
resin?
If the former, you have a glass supplier problem (not all the weaving
assistant burned off?)-- if the latter, then I would suspect incorrect
pH in the
adhesion promoter application bath.


Bill  Kenyon
Global Centre Consulting
3336 Birmingham Drive
Fort Collins, CO  80526
Tel: 970.207.9586   Cell:  970.980.6373

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2