Ted,
Thanks! That's one of the uses I remember for the term. That's closer to
the term for it from way back in my Plastic days. I will address the
need to revisit it in IPC-T-50.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ted Edwards
Sent: Monday, May 12, 2008 7:52 PM
To: [log in to unmask]
Subject: Re: [TN] The meaning of "skived"
Hi Dewey;
Before you leap a tall building in a single bound here is another use of
the
word skived. Skived is a term used in flex circuits fabrication to
define
how to clear covercoat and adhesive squeeze out of the pads a so that
the
pad will take solder. You skive the pads.
Ted Edwards
--------------------------------------------------
From: "Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Sent: Thursday, May 08, 2008 12:16 PM
To: <[log in to unmask]>
Subject: Re: [TN] The meaning of "skived"
> I am already pushing for some other changes to IPC-A-600 and this is
> IMHO an incorrect usage of the term. I am not sure of the time frame,
> but we'll get to yours briefly.
> Dewey
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Genny Gibbard
> Sent: Thursday, May 08, 2008 11:46 AM
> To: [log in to unmask]
> Subject: Re: [TN] The meaning of "skived"
>
> So which ones of you are on the IPC-A-600 committee?
> You can consider editing this for the next rev. Because "skived" is
the
> word used.
>
> Have a good day, eh? (from another Canadian)
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey
> (EHCOE)
> Sent: May 8, 2008 12:00 PM
> To: [log in to unmask]
> Subject: Re: [TN] The meaning of "skived"
>
> I am more used to the term skiving as it relates to compliant pins
being
> pushed into Tin-lead plated-through holes. The skiving results in FOD.
> I think thieving is more in-line with what you are referring to.
> Dewey
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Genny Gibbard
> Sent: Thursday, May 08, 2008 10:34 AM
> To: [log in to unmask]
> Subject: [TN] The meaning of "skived"
>
> Can anyone define "skived" as in:
> IPC-A-600 2.9.3.3 Ball Grid Array (Solder Dam)
>
> "....in order to avoid solder being skived from the attachment joint
> into the via."
>
> Online dictionaries define skive as: to slice off (leather, rubber,
> etc.) in thin layers; shave.
>
> It sort of gives me an idea, but it really isn't very clear.
> Thanks in advance.
>
> Genny
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
or
> (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
> per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100
> ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text
> in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100
> ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text
in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
[log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|