Craig,
I agree with Rex. As we were transitioning to lead free we went from
fully leaded to tin/lead boards with BGAs that were lead free to lead
free with a couple of tin/lead parts to fully lead free. For scenario
two we used what we called internally our "hot lead" reflow profile -
AFTER checking with all of our component manufacturers to make sure we
weren't going to cook anything.
Bev
RIM
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Rex Waygood
Sent: Thursday, May 01, 2008 10:01 AM
To: [log in to unmask]
Subject: Re: [TN] Pb-Free BGAs on a SnPb board
We run a profile that is known to achieve a full melt of the lead free
BGA balls (by section). The melting point of the ball is influenced by
the lead in the molten solder so the temperature required to achieve a
complete melt is lower than you might expect. On our boards the slight
increase in temperature is regarded as safe for the remaining
components. The boards have subsequently been through qualification
without failure. Our customer was involved fully with the investigation
and decision.
There is an NPL paper which also demonstrates this produces a reliable
BGA joint, under the conditions they checked :-).
Rex
Rex Waygood
Technical Manager
PartnerTech Poole Ltd
Benson Road
Poole
Dorset BH17 0RY
United Kingdom
Tel: +44 (0)1202 674333
Fax: +44 (0)1202 678028
DDI: +44 (0)1202 338222
Mob: +44 (0)7887 997403
[log in to unmask]
www.PartnerTech.co.uk
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Craig Sullivan
Sent: 01 May 2008 14:30
To: [log in to unmask]
Subject: [TN] Pb-Free BGAs on a SnPb board
Good Morning,
We are seeing an increased number of our customers that specify a
Pb-Free BGA when the rest of the board assembly is SnPb. Of course when
we reflow at the SnPb profiles, we don't always get a properly collapsed
BGA. So we end up reworking the BGA. We don't run a Pb-Free profile
because we don't want to risk damaging the SnPb components.
I am sure we aren't the only ones that are experiencing this. So, I have
a question or two:
What is everyone else doing when a customer requires a Pb-Free BGA on a
SnPb assembly? Many of the jobs I refer to are consignment, so it's not
like we can order the SnPb part from the get go.
What reliability issues do you see?
Are there any extra steps that your company takes to ensure the Pb-Free
BGAs collapse properly?
Is there a "special" profile anyone uses for the best of both worlds?
What are the advantages, if any, to use a Pb-Free BGA on a SnPb
assembly?
Thanks for any and all input.
Craig Sullivan
Manufacturing Engineer
MPL Incorporated
P: 607.266.0480
F: 607.266.0482
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
------------------------------------------------------------------------
-------
The information contained within this e-mail and any attachments
contained therein may be confidential and/or legally privileged and is
for the use of the intended recipient only. If you are not the intended
recipient please delete it from your system and notify the sender by
return e-mail. The content of this e-mail may not be copied or disclosed
to any third parties without prior permission from the sender.
E-mail is susceptible to data corruption, interception, tampering and
viruses. We do not accept any liability for any such incidents or any
consequences thereof.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|