Have Scotty teleport it and do a spectral analysis on the receiving end.
hey, it's friday...
At 09:53 AM 5/2/2008, Bev Christian wrote:
>TechNetters,
>I have a customer who wants to know the composition of any materials (if
>any) inside copper plated internal microvias. Obviously traditional
>x-sectioning would lead to contamination by the x-sectioning process.
>Someone suggested laser cutting, but that is ridiculous, for the same
>reason. Someone else suggested FIB, but this is fiendishly expensive,
>especially for the kind of depth of cut we might be talking about here.
>
>Any and all non-Friday afternoon suggestions welcome.
>(This last statement will probably backfire on me!)
>Bev
>RIM
>
>---------------------------------------------------------------------
>This transmission (including any attachments) may contain
>confidential information, privileged material (including material
>protected by the solicitor-client or other applicable privileges),
>or constitute non-public information. Any use of this information by
>anyone other than the intended recipient is prohibited. If you have
>received this transmission in error, please immediately reply to the
>sender and delete this information from your system. Use,
>dissemination, distribution, or reproduction of this transmission by
>unintended recipients is not authorized and may be unlawful.
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|