We recently qualified a SMT power module which has a small QFN part on the
board bottom side £¨the QFN package is intersil ISL6522 5mm¡Á5mm£©.
After the module was soldered to our board, We often found solder jointer
open in QFN terminal for remelting
We also find one doubtful point, in general, if the standoff of QFN has
obviously height and the solder jointer has beautiful fillet,
The module will easily have the open issue after reflow.
So we think the problem reason is caused from the incoming parts PCBA
process control and DFM design although the incoming is good,
Also we think the standoff of QFN in module should be controlled, otherwise
the solder jointer will have open issue in our PCBA.
Who have encountered the same issue or could give me any idea? Thanks in
advance!
Min Jun
H3C process engineer
Tel:+86-010-82774234
****************************************************************************
***********
This e-mail and its attachments contain confidential information from H3C,
which is intended only for the person or entity whose address is listed
above. Any use of the information contained herein in any way (including,
but not limited to, total or partial
disclosure, reproduction, or dissemination) by persons other than the
intended recipient(s) is prohibited. If you receive this e-mail in error,
please notify the sender by phone or email immediately and delete it!
****************************************************************************
************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|