TECHNET Archives

May 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 1 May 2008 11:03:41 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
"David D. Hillman" <[log in to unmask]>
X-cc:
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (138 lines)
Hi folks! Ok, here is the science: Gold dissolves  into a Sn60Pb40 solder 
bath 1 um (40 uinches) per second at 200C (W. Bader's data). So at 500F 
(260C) you increase the dissolution rate to over 4um (160 uinches) per 
second.  Contrast those dynamics with these elements using a Sn60Pb40 
solder bath :  Palladium dissolves at 1 um per second at 400C:  Nickel 
dissolves at 1 um per second over 500C! 

Dave Hillman
Rockwell Collins
[log in to unmask]



Werner Engelmaier /* <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
05/01/2008 10:15 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]


To
[log in to unmask]
cc

Subject
Re: [TN] De-golding?






Hi Dean,
No science--it just works.? Actually, any T above the Liquidus of solder 
will work, higher T's will work faster.

Werner


-----Original Message-----
From: Stadem, Richard D. <[log in to unmask]>
To: [log in to unmask]
Sent: Thu, 1 May 2008 11:01 am
Subject: Re: [TN] De-golding?



Good question. We use 500 deg. F. because we run our wave solder at 500
deg. F. and because 500 degrees F. is what we have been tinning at for a
long, long time, at least since the late 60's. I have no idea whether
that is the optimum temperature for dynamic wave tinning or not. I do
know that at least 9 companies in the Minnesota area, three in North
Dakota, and two in South Dakota all tin their parts at 500 deg. F. also.
I'm sorry I cannot tell you the science behind that temperature.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Braddock, Iain
Sent: Thursday, May 01, 2008 9:32 AM
To: [log in to unmask]
Subject: [TN] De-golding?

Apologies if this has found its way through before, I got an error
sending message from TechNet.
 
What temperature do you use for your SnPb de-golding pots and what is
the reason for your particular choice?
 
CIA,
    Iain


********************************************************************
This email and any attachments are confidential to the intended
recipient and may also be privileged. If you are not the intended
recipient please delete it from your system and notify the sender. You
should not copy it or use it for any purpose nor disclose or distribute
its contents to any other person. 

MBDA UK Limited, a company registered in England and Wales, registration
number 3144919 whose registered office is at Six Hills Way, Stevenage,
Hertfordshire, SG1 2DA, England.
********************************************************************

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for 
additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2