"Maybe we should have more community "case studies", I find the group
feedback to be very educational, especially when the descriptions in
IPC-A-600 are vague"
http://defectsdatabase.npl.co.uk/
Rex Waygood
Technical Manager
PartnerTech Poole Ltd
Benson Road
Poole
Dorset BH17 0RY
United Kingdom
Tel: +44 (0)1202 674333
Fax: +44 (0)1202 678028
DDI: +44 (0)1202 338222
Mob: +44 (0)7887 997403
[log in to unmask]
www.PartnerTech.co.uk
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson
Sent: 20 May 2008 15:36
To: [log in to unmask]
Subject: Re: [TN] Blue Voids
Well, since our supplier hadn't seen this condition in their
microsections, and the independent lab used different equipment
(Scanning Electron Microscope and Differential Interference Contrast
photography), the question became whether the supplier's lab could even
see the condition if it was present.
The independent lab still has the sample panel with the known condition,
and they agreed to send back half of the panel so the supplier can
experiment with it.
In the meantime, our company issued a corrective action request so we
get some kind of follow-up on the results.
Thanks to everyone who looked at the evidence and sent their opinion.
http://frontdoor.biz/PCBportal/bluevoid.jpg
p.s. I think its kind of fun to do this (especially when it is not MY
company's sample) .
Thanks again.
onward thru the fog,
Jack
-----Original Message-----
What became of this issue? I have not seen any more threads of e-mail.
Victor,
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: Tuesday, April 29, 2008 9:59 PM
To: [log in to unmask]
Subject: Re: [TN] Blue Voids
Are the voids in the glass bundle or between the glass bundle and the
resin?
If the former, you have a glass supplier problem (not all the weaving
assistant burned off?)-- if the latter, then I would suspect incorrect
pH in the adhesion promoter application bath.
Bill Kenyon
Global Centre Consulting
3336 Birmingham Drive
Fort Collins, CO 80526
Tel: 970.207.9586 Cell: 970.980.6373
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
-------------------------------------------------------------------------------
The information contained within this e-mail and any attachments contained therein may be confidential and/or legally privileged and is for the use of the intended recipient only. If you are not the intended recipient please delete it from your system and notify the sender by return e-mail. The content of this e-mail may not be copied or disclosed to any third parties without prior permission from the sender.
E-mail is susceptible to data corruption, interception, tampering and viruses. We do not accept any liability for any such incidents or any consequences thereof.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|