Correct me if I am wrong, is it depend on the layout? Like copper weight, tg, ground plane, etc. Much easy way to me is rent a high speed camera and get the true deflection by data. My silly 2 cents .
--------------------------
Sent using BlackBerry
----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Thu May 08 10:20:03 2008
Subject: Re: [TN] deflection data???
Look for an SMTA paper
"FLEXURAL STRENGTH OF BGA SOLDER JOINTS WITH ENIG SUBSTRATE
FINISH USING 4-POINT BEND TEST" SMTA Pan Pacific
Microelectronics Symposium, Kauai, HI, Jan. 25 – 27, 2005
At 07:03 AM 5/8/2008, Dan Skweres wrote:
>Good day all!
>I have received an inquiry from a customer
>regarding deflection data. They want to know if
>there's any data they can input so they can
>simulate if their BGAs will be ejected off their
>PCBs in a high vibe environment. The PCB is a 14
>layer FR-4 .062 thick. Any guidance would be greatly appreciated.
>Thanks,
>Dan S.
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of
>Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts:
>send e-mail to [log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach
>Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
|