At 08:34 AM 5/27/2008, Wenger, George M. wrote:
>I'm having a hard time believing that the size of the ho
>Robert,
concur. should be the opposite. Think about what "immersion" means
and how an immersion process behaves as the base metal is covered up.
>I'm having a hard time believing that the size of the hole has anything
>to do with Immersion Silver.
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Croslin, Robert
>Sent: Tuesday, May 27, 2008 10:57 AM
>To: [log in to unmask]
>Subject: [TN] PTH's With Immersion Silver
>
>We've been using immersion silver on our boards for quite a while with
>great success, but in a recent run of a new product, we had the boards
>come in with the PTH's used to mount RCA and audio connectors smaller
>that usual. The parts came in on the large end so it became very
>difficult for the operator to insert them into the board. Both holes
>and parts were in tolerance and the holes were specified at the
>recommended diameters. Our CM has a woman who spent 20 years working in
>pcb fab houses and she tells me that it's not at all unusual to have IS
>boards with reduced ID's on the holes as opposed to HASL. Has anyone
>else experienced this? If this is the case, we'll have to adjust for
>this in the future, but it would be useful to know if this was an
>anomaly or a normal condition?
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text
>in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at:
>http://listserv.ipc.org/archives
>Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
>ext.2815
>-----------------------------------------------------
>
>
>No virus found in this incoming message.
>Checked by AVG.
>Version: 8.0.100 / Virus Database: 269.24.1/1468 - Release Date:
>5/26/2008 3:23 PM
>------------------------------------------------------------------------------------------------
>This message is for the designated recipient only and may
>contain privileged, proprietary, or otherwise private information.
>If you have received it in error, please notify the sender
>immediately and delete the original. Any unauthorized use of
>this email is prohibited.
>------------------------------------------------------------------------------------------------
>[mf2]
>
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|