Ioan,
Well at least there are no fully fluorinated materials. The two HFC have global warming potentials, but I don't have the numbers on me. (am in a meeting. :) ). You will have to decide how big a GWP you are comfortable with.
Methanol is of course flammable and has a significant TLV - thus explaining blindness and death for those that drink it.
The race car guys can tell you about the nitromethane.
Make sure this stuff is used with adequate ventilation. Some HFCs are flammable. Some are not. It depends on the hydrogen/fluorine ratio. Their type and amount will also affect how susceptible the methanol is to a spark.
Bev
RIM
----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Wed May 21 12:04:42 2008
Subject: [TN] Are these substances OK for use in electronics
Dear Technos,
I've got one for the chemists: a customer of ours requests us to clean
their boards with 2 spray canned products. Here's the stuff that's
inside of them:
1,1,1,2,3,4,4,5,5,5-Decafluoropentane
Trans,1,2-Dichloroethylene
Methanol
Nitromethane
1,1,1,2-Tetrafluoroethane
Are they safe for the product? What about the production personnel and
the environment?
Thanks,
Ioan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|