Using a Gerber software package and the CAD files you can get the area
of the stencil layers of each board style. Knowing the thickness and
area and density of solder paste you can determine the volume of paste-
most pastes are 50 pbw. Assume that paste transfer is complete.
(Stencil area x stencil thickness)/ solder paste density = gms of solder
paste
First pass approximation but there are so many variations in area and
board size that if makes it difficult to come up with an average value.
Tom
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dan Mathews
Sent: Tuesday, May 20, 2008 12:10 PM
To: [log in to unmask]
Subject: [TN] Average paste volume estimate
Does anyone have an easy way to estimate how much paste is applied to a
smt pcb? I understand it varies on
squeegee pressure, stencil thickness, and pitch of the components but I
was looking for an average. I would
assume that somewhere out there someone can estimate that "2 grams of
paste is used on a 2" x 2" smt pcb".
I will then use this information to determine how much lead is used on
non-RoHS products due to solder paste
issues and not non-compliant components.
Thank You in Advance,
Dan
Dan Mathews C.I.D.+
Engineering Support Supervisor
B&B Electronics
Ottawa, IL USA 61350
Phone: 815-433-5100 ext 217
Fax: 815-434-8831 (direct to my desk)
URL: http://www.bb-elec.com <http://www.bb-elec.com/>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|