I'm just wearing brief moments of lucidity. Well, and some jeans - it
being Friday and all.
regards,
- Graham
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
Sent: Friday, May 16, 2008 3:17 PM
To: [log in to unmask]
Subject: [TN] NTC RE: [TN] The meaning of "skived"
You have technical briefs? Gee, I've been wearing legal briefs. I'm
gonna have to git me some of them technical briefs.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey
(EHCOE)
Sent: Friday, May 16, 2008 12:09 PM
To: [log in to unmask]
Subject: Re: [TN] The meaning of "skived"
Technical Briefs are one of the pluses of this forum. How ironic I was
looking into a wedge void problem.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Randy Bock Sr.
Sent: Friday, May 16, 2008 8:47 AM
To: [log in to unmask]
Subject: Re: [TN] The meaning of "skived"
Oh what memories....
Randy Bock Sr.
Quality Engineer
Enterprise Quality Assurance
AddressRight Printers
(email) [log in to unmask]
Newtown Building 2
203 270-4931 Ext
8-426-4931 In
203 270-4982 Fax
This e-mail message may contain confidential, proprietary and/or
privileged information. It is intended only for the use of the intended
recipient(s). If you receive this in error, please immediately advise
the sender by reply e-mail and delete this e-mail message. Any
disclosure, copying, distribution or use of the information contained in
the e-mail to or by anyone other than the intended recipient is strictly
prohibited.
Any
views expressed in this message are those of the individual sender,
except when the sender specifically states them to be the views of the
company.
Thank You.
Steve Gregory <[log in to unmask]> Sent by: TechNet
<[log in to unmask]>
05/16/2008 11:45 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to Steve Gregory
<[log in to unmask]>
To
[log in to unmask]
cc
Subject
Re: [TN] The meaning of "skived"
Hahaha! You just reminded me of my Navy days!
I remember going out in town to have few cool ones with my shipmates and
walking into a bar filled with marines, and being caught there when one
of the grunts yelled; "Skivy check"! Then wishing that I hadn't been
wearing them.
I just guess you had to be there...
(You sailors and Marines know what I'm talking about)
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ken Bloomquist
Sent: Friday, May 16, 2008 10:37 AM
To: [log in to unmask]
Subject: Re: [TN] The meaning of "skived"
I could have sworn that "skiving" was when you didn't have a bathing
suit and went swimming with just your skives on :-)
Happy Friday,
KennyB
-----Original Message-----
From: Simonik, Dave R. (David) [mailto:[log in to unmask]]
Sent: Friday, May 16, 2008 8:11 AM
To: [log in to unmask]
Subject: Re: [TN] The meaning of "skived"
We also use the term 'skived', but only in our laser drilling process.
The process of skiving in our facility is the use of the Uv laser to
skive down to inner layer alignment targets. This process of involves
continuous pulsing of the Uv laser, whereby a window is opened up on the
board. The process pulses the beam in a raster pattern, with shot and
line spacing set for the proper removal of material at high power and
low rep rate. The second step of the skiving process uses lower power at
a higher rep rate with expanded shot & line spacing to clean the copper
surface of remaining dielectric material in order that the vision system
can capture the imaged target.
Dave Simonik
Process Technician
Sanmina SCI
Owego NY PCB Division
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
Note: All the information contained in this e-mail and its attachments
is proprietary to Kaiser Systems, Inc. and it may not be reproduced
without the prior written permission of sender. If you have received
this email in error, please immediately return it to sender and delete
the copy you received.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|