TECHNET Archives

May 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Mon, 5 May 2008 16:17:23 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, R Sedlak <[log in to unmask]>
Subject:
From:
R Sedlak <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset=us-ascii
MIME-Version:
1.0
Parts/Attachments:
text/plain (52 lines)
Bogert:   You have asked one of those unanswerable questions.  
Or Kenny B quoted Dewey's famous "It depends".
Whereas in theory the consequences of leaving saponifier residue behind are dire, in fact, the real issue resolves around HOW MUCH residue you are talking about.  This being because as the saponifier residues are exposed to air and metals, they are neutralized, and the amount of metal oxide generated is a tiny fraction of the amount of saponifier left behind.
 My suspicion is that given a reasonable DI water rinse, the amounts left on the board would be trivial, and whereas one can never be perfectly certain, in fact I suspect that the implications would not be noticeable.

Always remember free advice is often not worth what you paid for it...

Rudy Sedlak
RD Chemical Company.

--- On Mon, 5/5/08, - bogert <[log in to unmask]> wrote:
From: - bogert <[log in to unmask]>
Subject: [TN] Saponifier residue
To: [log in to unmask]
Date: Monday, May 5, 2008, 3:00 PM

May 5, 2008

I have the following question:  If a saponifier is used with a DI cleaning 
machine to clean PWAs and the cleaning does not remove all traces of the 
saponifier, is there any concern, including sugsequent exposure, to a humid 
environment?  Any technical reports on this subject?

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


      ____________________________________________________________________________________
Be a better friend, newshound, and 
know-it-all with Yahoo! Mobile.  Try it now.  http://mobile.yahoo.com/;_ylt=Ahu06i62sR8HDtDypao8Wcj9tAcJ

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2