Some types of solder mask contain nasties that may prevent a decent
adhesion of a CC or they may not have been properly polymerised, leaving
insoluble monomers or other components on the surface. I suggest you
start looking in this direction.
Brian
Phil Nutting wrote:
> We are using Chemtronics Konform AR on some circuit boards. The boards are batch washed in DI water and pre-baked prior to coating and then cured in a 60° or 77° C oven.
>
> In a recent test of a new washing system where we are removing slip ring dust (brass and carbon) on these boards and dielectric oil from other boards and aluminum castings, I noticed the conformal coating peeling off in sheets after both the wash and DI rinse cycles. Both wash and rinse are between 140 and 150° F.
>
> Is this stuff peeling off because of the water temperature, poor pre-coating prep or possibly something else?
>
> Thanks in advance,
>
> Phil
>
> Note: All the information contained in this e-mail and its attachments is proprietary to Kaiser Systems, Inc. and it may not be reproduced without the prior written permission of sender. If you have received this email in error, please immediately return it to sender and delete the copy you received.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|