TECHNET Archives

May 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Ioan Tempea <[log in to unmask]>
Date:
Thu, 22 May 2008 14:45:43 +0300
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
From:
Brian Ellis <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset=ISO-8859-15; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (96 lines)
OK, the HFCs are severe greenhouse gases, with GWPs of 300-1500 (CO2=1) 
and are controlled substances under the Kyoto Protocol. They are not 
aggressive cleaning solvents and, by themselves, are not good flux 
removers. They are almost non-toxic. They should not be used near 
soldering equipment as pyrolytic decomposition may occur at >200°C and 
the resultant by-products are VERY toxic (carbonyl fluoride and hydrogen 
fluoride).

The trans-DCE is quite similar to trichloroethylene and is fairly toxic: 
it is added to make the mix a better solvent for oils and greases. This 
was used in preference to other chlorocarbon solvents because it is the 
only one for which OSHA do not have an official PEL, as epidemiological 
studies on its toxicity have not been conducted: it is therefore in that 
legal limbo where manufacturers can suggest their own exposure limits 
which may or may not be safe. Because it is a lot cheaper than HFCs, it 
tends to pull the price of the blend down. It is hardly ozone-depleting 
and is not a controlled substance. It attacks many plastics.

The methanol is added to widen the dissolution spectrum and to improve 
the dissolution of rosin and some organic ionic materials. It is highly 
toxic and damages the central nervous system and the damage is 
cumulative. It is very easily absorbed through the skin, as well as by 
respiration (hopefully not to be ingested!). Of course it is flammable.

The nitromethane is a stabiliser to prevent the trans-DCE from 
hydrolysing into hydrochloric acid. Normally, it would be present in 
very small quantities. It is violently flammable and toxic, but this is 
not your worry.

The use of spray cans to achieve good cleaning is very difficult. 
Normally, you will have to hold the board at about 45° from the 
horizontal (coincidentally, about 45° to the vertical, as well!!!!) and 
spray the area to be cleaned very liberally, until the liquid well and 
truly starts to stream off the edge of the board. Pause a few tens of 
seconds and repeat n times (n >5), until the desired level of 
cleanliness is achieved. Never allow the solvent to dry on the board, as 
this will just spread the residues where they will cause more harm than 
if you had not tried to clean in the first place. Spray cans, used 
properly, are an expensive cleaning method.

Brian

Ioan Tempea wrote:
> Dear Technos,
> 
>  
> 
> I've got one for the chemists: a customer of ours requests us to clean
> their boards with 2 spray canned products. Here's the stuff that's
> inside of them:
> 
> 1,1,1,2,3,4,4,5,5,5-Decafluoropentane
> 
> Trans,1,2-Dichloroethylene 
> 
> Methanol
> 
> Nitromethane
> 
> 1,1,1,2-Tetrafluoroethane
> 
>  
> 
> Are they safe for the product? What about the production personnel and
> the environment?
> 
>  
> 
> Thanks,
> 
>  
> 
> Ioan
> 
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2