Good Morning,
We are seeing an increased number of our customers that specify a Pb-Free
BGA when the rest of the board assembly is SnPb. Of course when we reflow at
the SnPb profiles, we don't always get a properly collapsed BGA. So we end
up reworking the BGA. We don't run a Pb-Free profile because we don't want
to risk damaging the SnPb components.
I am sure we aren't the only ones that are experiencing this. So, I have a
question or two:
What is everyone else doing when a customer requires a Pb-Free BGA on a SnPb
assembly? Many of the jobs I refer to are consignment, so it's not like we
can order the SnPb part from the get go.
What reliability issues do you see?
Are there any extra steps that your company takes to ensure the Pb-Free BGAs
collapse properly?
Is there a "special" profile anyone uses for the best of both worlds?
What are the advantages, if any, to use a Pb-Free BGA on a SnPb assembly?
Thanks for any and all input.
Craig Sullivan
Manufacturing Engineer
MPL Incorporated
P: 607.266.0480
F: 607.266.0482
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|