TECHNET Archives

May 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
ipC Technet <[log in to unmask]>
Date:
Tue, 20 May 2008 16:54:23 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Leif Erik Laerum <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Subject:
From:
Leif Erik Laerum <[log in to unmask]>
Content-Type:
text/plain; charset=ISO-8859-1; format=flowed
In-Reply-To:
Organization:
Texas Memory Systems
MIME-Version:
1.0
Parts/Attachments:
text/plain (35 lines)
All,

Thanks for all the suggestions. We will definitely run some experiments. 
I am glad I got some confirmation on my oxidation theory.

The traces on the side does not really follow what we observe on the 
board. The cooling issue is something we have discussed as well. This is 
a well established design that has not undergone any changes other that 
moving the 0402 pads closer together. The caps were shifting on the 
previous rev as well, but that was more due to that the pads were too 
far apart and the pad on the components was not always 100% on the pad. 
The shifting was straight and in the direction of one of the pads. We 
have now solved this issue, but got the turning one instead.  If this 
was a cooling issue and/or a surface tension issue we would have had the 
same issue of previous rev boards. The change is in this capacitor.

I will keep you posted.

Leif Erik Laerum
Quality Assurance Manager
Texas Memory Systems
[log in to unmask]
Tel: (713) 266-3200 x468
www.texmemsys.com

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2