TECHNET Archives

May 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Tue, 13 May 2008 11:34:14 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Leland Woodall <[log in to unmask]>
Subject:
From:
Leland Woodall <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (131 lines)
Bruce,

Thus far, they've only been found on the top side of our products.  Our
boards carry several .5 mm pitch ICs there, and yes, those are the only
locations that have been identified with this condition.

To my knowledge, all of our ICs come directly from their respective
manufacturers.  In rare cases we use brokered components, but those have
been typically limited to chip resistors and caps.

Leland

-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]] 
Sent: Tuesday, May 13, 2008 11:21 AM
To: [log in to unmask]; Leland Woodall
Subject: RE: [TN] Stainless Steel Contamination Question


Leland,

You said they occur on top of the .5 mm pitch ICs. That's curious.
 
Are you finding them anywhere else on the board, or just at those
specific IC locations?  

Is this a problem on just one side of the board?

Any chance these are broker parts and the strands are in already on the
parts? There can be all kinds of strange debris in some of that
material.

Bruce Tostevin
Benchmark Electronics
Hudson, NH


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall
Sent: 13 May 2008 14:47
To: [log in to unmask]
Subject: [TN] Stainless Steel Contamination Question
Importance: High

Hi Everyone,

 

We've had a problem lately with fine strands of stainless steel wire
being found on top of some of our .5 mm pitch ICs.  This
has caused both internal and external issues, and we've yet to identify
the source.

 

It's definitely formed wire, with a thickness ranging from 7 to 10
microns, and up to 3 mm in length.  

 

Our automated optical inspection stations can only reliably detect
widths of 12 to 15 microns.

 

I've checked the internet in an attempt to find common applications of
this wire.  I've found two, and they were for ultra-fine
filters and stencil screen mesh.  We've investigated (I think) all of
our machinery that would utilize filters this small and
have found no such usage.
I've also checked every stencil in our plant, and all of our mesh
material is some type of a plastic compound.

 

Do you have any idea where this stainless steel might be coming from?

 

Any suggestions would be sincerely appreciated!

 

Thanks,

 

Leland


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with
following text in the BODY (NOT the subject field): SIGNOFF Technet To
temporarily halt or (re-start) delivery of Technet send
e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE
mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest Search the archives of previous
posts at: http://listserv.ipc.org/archives Please visit IPC
web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at
[log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2