Subject: | |
From: | |
Reply To: | |
Date: | Wed, 16 Apr 2008 18:51:28 +0100 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
Same date code does not necessarily mean the same batch of boards.
Its simple to test the boards this procedure has been posed before to test
the board and so have the video clips on what you may see to tell if it's
the boards or not.
Outgassing testing of boards the Bob Willis way
www.bobwillis.co.uk/video/outgassing.wmv
This is a ? out of the 10 performance
www.bobwillis.co.uk/videoclips/outgassing01.wmv
This is a ? out of 10
www.bobwillis.co.uk/videoclips/outgassing02.wmv
Its not just boards that do it!!
www.bobwillis.co.uk/videoclips/outgassing5.wmv
Test method www.bobwillis.co.uk/outgass.rtf
Many thanks
Bob Willis
2 Fourth Ave, Chelmsford, Essex, CM1 4HA England
Tel: (44) 1245 351502
Fax: (44) 1245 496123
Mobile: 07860 775858
www.ASKbobwillis.com
Book your place on Bob's "Step by Step Failure Analysis Workshop" 14th May
www.ASKbobwillis.com/faworkshops.pdf
New "Printed Board Inspection & Quality Control" 3 July
www.ASKbobwillis.com/PCBworkshop.pdf
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ken Bloomquist
Sent: 16 April 2008 18:03
To: [log in to unmask]
Subject: [TN] Out Gassing
No sooner do I get back and I need some help. This is an age old subject
that has once again reared its ugly head.
We have an assembly that we are building with mixed technology. We have a
kit for several thousand and we release them in work orders of 250. All of
the PWB's have the same date code 3307. We process about 500 a day.
The first 250 went through without a hitch; the second 250 had a few pin
holes in the through-hole components; the last 250 were terrible with what
I'd call severe out gassing on 50 out of 250.
What the heck would cause a drift like that from Tuesday to Wednesday?
Thank,
KennyB
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest