Not enough high mag to discern details of the polish surface and
condition of glass rods.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson
Sent: Monday, April 28, 2008 10:03 PM
To: [log in to unmask]
Subject: [TN] Blue Voids
Greetings!
Once again I am caught in the middle of a bare board problem,
(never the same thing twice!)
Maybe after a few more decades of failure I might become more
proficient at evaluation, but in the meantime....
Does anyone have a quick reaction to this picture?
http://frontdoor.biz/PCBportal/bluevoid.jpg
I'm told there are voids in the glass fiber bundles.
When I reported it to the manufacturer, they asked that blue
dye be applied to see the penetration. It all looks blue!
(and other areas look "bluer" than the problem area to me)
The description in IPC-A-600 is too brief to comprehend
and I can't find anything in Printed Circuits Handbook about it.
anyway,
I'm not doubting anything I've been told by "the experts",
my question is:
How would you handle this if you saw it in YOUR report?
reject?
use the boards but ask for corrective action?
process indicator but not really a problem?
not sure, but monitor with more xsec?
onward thru the fog,
Jack
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|