We do not use a tool to install the connectors. Actually the holes are sized
quite generously and the pins go in pretty easy. I don't have a force meter
so don't know what it actually takes but it's not much.
Like I said in my previous reply we never saw this before we started using
the selective solder pallets.
Thanks for your thoughts,
KennyB
---------------------------------------------------