Phil,
There are several manufacturers of this type of material, static dissipative
FRP. They are fairly expensive.
The manufacturer's I know of are:
Mfr: Permali
Mat'l: Durostone CAS761, Durostone CAG762
Mfr: Norplex Micarta
Mat'l: Wavemax 5000
Mfr: Vonn-Roll Isola
Mat'l: Durapol IGM-L200, Delmat CDM ESD 68940, Delmat DM ESD 68610
Most of these are sold through distribution only. I would contact the MFRs
for data-sheets and distributors near you.
However, I found that unless you buy standard sheet sizes, you pay even
more. When I was looking at buying direct to machine internally, prices
ranged from $100 / sq-ft all the way to $310 / sq-ft, which didn't make it
very cost effective. In my opinion, it is a much better deal to use a
tooling fab shop, such as the one Rich provided to you. There are others
also.
Kevin Glidden
Manufacturing Engineer
Luminescent Systems Inc.
-----Original Message-----
From: Phil Nutting [mailto:[log in to unmask]]
Sent: Thursday, April 17, 2008 8:25 AM
To: [log in to unmask]
Subject: [TN] Need recommended material for a wave profiling pallet
Good morning,
I have a profiler that I want to mount in/on a panel I can use repeatedly in
my wave solder machine. I've seen a white material, at ACI in
Philadelphia, used for other types of soldering pallets, but I have no
information on the material. Hopefully the material can be easily machined
without special equipment or tools.
Can someone point me to this material?
Thanks in advance.
Phil Nutting
Note: All the information contained in this e-mail and its attachments is
proprietary to Kaiser Systems, Inc. and it may not be reproduced without the
prior written permission of sender. If you have received this email in
error, please immediately return it to sender and delete the copy you
received.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|