Hi Terry,
The materials under these slash sheets may or may not be 'RoHS-compliant',
but with the exception of /99 they are not 'RoHS-capable'. That means that their
STII (Soldering Temperature Impact Index)-values are too low. /99 gives a
minimum STII of 202, which would make that material of limited usefullness for
lead-free soldering processes—there are however materials under slash /99 that
have higher STII values.
For more information—a lot more information—you should be getting my White
Paper: "Recommendations for PCB FAB Notes and Specifications in Printed Circuit
Board Drawings for SnPb and Lead-Free Soldering Assemblies, the Qualification
of PCB Shops and Activities to Assure Continued Quality."
Werner
**************
Need a new ride? Check out the largest site for U.S. used car
listings at AOL Autos.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------