I have been known to bake a small amount of boards in a regular oven (clean
well afterward and keep well ventilated to elevate any noxious gases).
Kat
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phil Nutting
Sent: Wednesday, April 16, 2008 12:39 PM
To: [log in to unmask]
Subject: Re: [TN] Out Gassing
Ken,
I remember a recent thread that talked about immersion tin being difficult
to wave solder after the reflow process. Had to do with oxidation due to
the heat of reflow. In this thread I don't recall what your board material
is, type of plating and type of solder.
Just a thought,
Phil
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ken Bloomquist
Sent: Wednesday, April 16, 2008 1:32 PM
To: [log in to unmask]
Subject: Re: [TN] Out Gassing
Kat,
I'm going to try and bake some but our oven only goes up to 140 degrees F.
I'm not sure if that will do much. Any idea how long you'd have to bake at
140 to do any good?
Richard,
The pinholes are on the through-hole components and come after wave solder.
By sever I mean about 80% of the through-hole leads exhibit out gassing. We
run hundreds of boards through our wave solder every day and this is the
only board we're seeing this on.
Steve,
We just changed the flux Monday and we do a SG check on it every morning to
keep it in balance.
Dewey,
Play Misty for Me :-)
Roger,
Don't go there even though I'm having five bean soup for lunch, ooh!
Thanks,
KennyB
-----Original Message-----
From: Kathy Kuhlow [mailto:[log in to unmask]]
Sent: Wednesday, April 16, 2008 10:08 AM
To: 'TechNet E-Mail Forum'; Ken Bloomquist
Subject: RE: [TN] Out Gassing
Ken,
What is the humidity been the last few days? Can you bake some and then
repeat the run to see if the outgassing continues? I have had PCB's that
when baked lost pin holes/blow holes.
Kat
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
Note: All the information contained in this e-mail and its attachments is
proprietary to Kaiser Systems, Inc. and it may not be reproduced without the
prior written permission of sender. If you have received this email in
error, please immediately return it to sender and delete the copy you
received.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|