You should refer to IPC-7711A/21A.
Regards,
Cliffz
-----Original Message-----
From: TGAsia [mailto:[log in to unmask]] On Behalf Of QC 王世奎
Sent: Thursday, April 17, 2008 4:51 PM
To: [log in to unmask]
Subject: [TGA] 烙铁使用
各位大侠:
小弟有一个问题请教一下,过完波峰焊后有贴片元件和散热片未焊的,有无那份标准
规定焊什么元件用什么样的烙铁,温度应该是多少?
谢谢各位大侠帮忙,小弟先谢谢各位.
==============================================================
Thanks & Best Regards!
QC 王世奎
E-mail : [log in to unmask]
Tel : (86) 010-64326699 Ext. 8323
Add : No.10 Jiuxianqiao Road,Chaoyang District,Beijing,China
地址 : 北京市朝阳区酒仙桥路10号
TPV Technology (Beijing) Co., Ltd. Quality Assurance Division
冠捷科技(北京)有限公司品保部
==============================================================
|
|
|