Hi Kenny!
Spent many days up there flying anti-submarine missions out of NAS
Whidbey back when I was a flight engineer in the Navy...a lot of Soviet
subs used to hang-out up at that part of the left coast.
Yeah, it's beautiful when it isn't raining. But you know what they say
about people from Washington state don't you? They don't tan, they
rust... ;^}
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: Wednesday, April 16, 2008 10:42 AM
To: [log in to unmask]
Subject: Re: [TN] Defects related to water wash
Kenny!!!!!!!!!
Welcome back,
Any jobs? My wife has always wanted to move there.....
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ken Bloomquist
Sent: Wednesday, April 16, 2008 8:06 AM
To: [log in to unmask]
Subject: Re: [TN] Defects related to water wash
Hi Everybody,
I've been away from the TechNet for a while but it's good to be back.
I'm now working for a wonderful EMS on beautiful Whidbey Island,
Washington.
Carl, you hit on a subject that we are addressing right now. We use
metal wire mesh baskets to transport assemblies through our wash. We
experience damaged SMT parts from time to time such as chipped caps or
missing parts.
We believe that it is from the water pressure and air pressure bouncing
the boards around and banging them into the wire mesh.
We are evaluating several different ideas but haven't found the best fix
yet. I'll be interested to hear if other TechNetters have this problem
and if so how they've solved it.
Best regards,
KennyB
-----Original Message-----
From: Ray, Carl (GE EntSol, Intelligent Platforms)
[mailto:[log in to unmask]]
Sent: Wednesday, April 16, 2008 7:48 AM
To: [log in to unmask]
Subject: [TN] Defects related to water wash
Does anyone out there have any information or data related to defect
rates for components after water wash processes? Some obvious components
such as switches, speakers and similar devices that are exposed to the
wash is a given to expect failures. The concern we have is with other
types of components.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|