Hi Wayne! Ah, if it were only that easy! A QFN component essentially is a
"blind solder joint" so you must rely on your process to produce an
acceptable solder joint and confirm that process consistency through
testing. We are faced with a variety of component styles now, such a
bottom only terminated devices, where there is no visible solder joint
available for inspection. Using a combination of process validation, Xray
inspection techniques and product integrity testing, you should be able to
confirm the solder joint integrity. A very common industry myth is that we
"inspect" quality into our electronic assemblies - the reality is that the
inspection step is only a confirmation that your design and assembly
processes are controlled/consistent. The JSTD-001 and IPC-610
specifications attempt to provide as much assistance as possible. Good
Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
Wayne Thayer <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
04/10/2008 09:35 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Wayne Thayer <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] FN Parts--Evidence of Wetting
Relevant IPC specs claim that no toe fillet is required for DFN/QFN parts
and
there is no minimum solder joint height. The only requirement for the
joint
other than alignment/pad size is "evidence of wetting". How do I get this
evidence without a toe fillet? I suppose if I have enough joint height I
can
see under the part like a BGA, but I've never seen a FN part mounted that
high.
Would be nice if the spec included some pix/examples of this "evidence".
Any recommendations would be very much appreciated.
Thanks,
Wayne Thayer
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|