Since the question was asked that way, there probably would be no issues
at the design level. If they were really concerned they would have
specified the printed board (PB) per IPC-6012, Class 2 or 3 or by using
the appropriate alpha-numeric designators in the procurement section.
IPC-A-600 just establishes acceptability for PBs.
The difference between Class 2 and Class 3 of IPC-6012 from a design
standpoint is minimal and may only be pertinent if you were pushing the
limits.
A sidebar to this is if a designer were fully responsible for the
deliverable, I have always felt that it was his responsibility to
establish that his designs were built on a good foundation. The basic
difference between Class 2 and 3 is you can say you're 2, but must prove
you're 3. PBs built to Class 3 of IPC-6012 gives the designer an
expectation of the basic requirements of a good foundation for his
designs.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Collins
Sent: Monday, April 14, 2008 6:02 AM
To: [log in to unmask]
Subject: [TN] PWB spec Class 2 vs assembly spec Class 3
Good day 'Netters
A hypothetical question.
If a PWB is specified to IPC-A-600 class 2, and the assembly is
specified to IPC-A-610 class 3, does this cause any issues for assembly?
We have a new designer who claims it would cause no problems, I am not
familiar with IPC-A-600 so can't offer a valid opinion.
Thanks!
Graham Collins
Halifax Production Engineering
L-3 communications Electronic Systems
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|