TECHNET Archives

March 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Joe Russeau <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Joe Russeau <[log in to unmask]>
Date:
Wed, 5 Mar 2008 13:56:18 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (203 lines)
Hi Chris,

I hope you don't mind my diving into this question.  We often recommend 
somewhere in the 2-10 Megohm-cm range for deionized water assembly cleaning, 
with 5-6 megohm being sort of the target.  Keep in mind that there is no one 
size fits all answer, as there are several "it depends" factors here.   I am 
assuming, based on your question,  that you have not studied the effects of 
varying the water resistivity.  That being said, data is always king. 
Perhaps doing some studies varying the water resistivity would give you the 
answer you seek.

As for why you continue having cleaning concerns, could it be that deionized 
water alone doesn't pack enough of a punch to get the job done consistently? 
Residues are always a compilation of bare boards, components, and assembly 
materials.  Any variation in the consistency of their cleanliness and normal 
assembly process variation can yield variations in the cleaning results. 
Understanding those variations would help you better define what cleaning 
parameters need to be tweaked to achieve a more robust and consistent 
cleaning process.

Just my 2 cents.

Best Regards,

Joe Russeau
Process Analyst

Precision Analytical Laboratory, Inc.

----- Original Message ----- 
From: "Schaefer, Chris" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, March 05, 2008 11:43 AM
Subject: Re: [TN] Cleaning No-clean


Terry,

A little off the subject. How important do you think it is to use high 
quality DI water as opposed to using 200K DI water in an Inline Aqueous 
System? I typically use something in the range of 12-18Mohm DI water at a 
minimum at the final rinse whether its a chemistry inline wash or purely a 
water wash. We produce Class 3 product that requires zero residuals at 
10-40X, with less than 10.06NaCl/ sq.in. ionics. The company I am currently 
working for does not believe 10-18Mohm water is necessary, but we continue 
to have cleaning issues that are caused by poor process, old chemistry, and 
likely the water.

Any thoughts?

Thank You,

Chris - AKA Booker



Chris Schaefer
Suntron Corporation
Process Engineer

800 N. Brutscher Street
Newberg, OR 97132
Work Phone: 503.554.6270
Cell Phone: 785.248.9016
Email: [log in to unmask]

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Terry L. Munson
Sent: Wednesday, March 05, 2008 8:22 AM
To: [log in to unmask]
Subject: Re: [TN] Cleaning No-clean

Dan and Brian
We have qualified clients who clean a no clean and have since the mid 90's 
(Les Hymes was one of the first). But we have found that with a rescue 
cleaning  and only if you have water tolerant parts (if not those need to be 
removed) that  you can effectively clean a residue that was not designed to 
be cleaned.
  These residues do need a good saponifier, low pressure inline (not able to 
do in  a standard batch system), heated to 140-150 F wash and rinse with DI 
water at 10  meg ohm or better, but this is not enough by itself but we 
found that if we use  DI steam after wash and before rinse then we are able 
to clean under low  standoff components, BGA's, and with a little help QFN 
and PQFN
packages.   We presented this information at the IPC Midwest Expo 2007, 
authored
by  Eric Camden.  We have successfully been rescue cleaning for the last 7 
years no clean assemblies that were 6-12 months old.  So it is very doable 
but standard batch cleaning with a saponifier has not proven to us or our 
customers who we have help implement this type of cleaning that batch or 
standard inline cleaning is able to do the job.

Terry Munson
Foresite
765-457-8095




In a message dated 3/5/2008 10:53:25 A.M. Eastern Standard Time, 
[log in to unmask] writes:

"Generally speaking I have not seen good results in trying to clean  off 
no-clean flux. They call it "no-clean" for a reason."

Agreed!!!  Even if you succeed to do the job well - it can be done with some 
fluxes -  it will not be very easy and may be quite costly. I have always 
said, if  you clean, use a flux which was designed from the start for easy 
cleaning.

¤0.02 worth

Brian

Dan Mauro wrote:
>  Folks,
>
>
>
> I have a need to clean  No-clean residue from PCBA's. Can this be
> achieved with water washer  and some type of saponifier ? Can anybody
> suggest a batch  process?
>
>
>
> Thanks,
>
>  Dan
>
>
>  ---------------------------------------------------
> Technet Mail List  provided as a service by IPC using LISTSERV 15.0 To
> unsubscribe, send  a message to [log in to unmask] with following text
> in the BODY (NOT the  subject field): SIGNOFF Technet To temporarily
> halt or (re-start)  delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or  (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous  posts at:
> http://listserv.ipc.org/archives Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information,  or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
>  -----------------------------------------------------
>

---------------------------------------------------
Technet Mail  List provided as a service by IPC using LISTSERV 15.0 To 
unsubscribe, send  a message to [log in to unmask] with following text in the 
BODY (NOT the  subject field): SIGNOFF Technet To temporarily halt or 
(re-start) delivery  of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To  receive ONE mailing per 
day of all the posts: send e-mail to
[log in to unmask]:  SET Technet Digest
Search the archives of previous posts at:  http://listserv.ipc.org/archives 
Please visit IPC web site  http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information,  or contact Keach Sasamori at [log in to unmask] or 
847-615-7100  ext.2815
-----------------------------------------------------




**************It's Tax Time! Get tips, forms, and advice on AOL Money &
Finance.      (http://money.aol.com/tax?NCID=aolprf00030000000001)

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
unsubscribe, send a message to [log in to unmask] with following text in the 
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or 
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet 
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send 
e-mail to [log in to unmask]: SET Technet Digest Search the archives of 
previous posts at: http://listserv.ipc.org/archives Please visit IPC web 
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional 
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2