I suppose you can screw up any process if you do not control it. I have been
involved in many long term applications of flash gold and there have been no
problems. Obviously, if you are having Au embrittlement, the coating is not
flash gold which by every definition I am familiar with is 3 micro inches or
less.
Best regards
Lee
J. Lee Parker, Ph.D.
JLP Consultants LLC
804 779 3389
----- Original Message -----
From: "Werner Engelmaier /*" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, March 28, 2008 7:21 PM
Subject: Re: [TN] Gold Flash vs. ENIG Solder finish
> Hi Lee,
> However, I have been involved in issues of Au-embrittlement as a
> consequence
> of the electrolytic flash gold being plated too thick.
>
> Werner
>
>
>
> **************
> Create a Home Theater Like the Pros. Watch the video on AOL
> Home.
> (http://home.aol.com/diy/home-improvement-eric-stromer?video=15&
> ncid=aolhom00030000000001)
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|