In Mask defined BGA pads; is the mask surface higher than the BGA pad surface?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Thayer, Wayne
Sent: Tuesday, March 18, 2008 7:20 AM
To: [log in to unmask]
Subject: Re: [TN] Solder Mask Defined Pad BGA Reliability
Buy any BGA built on glass composites and turn it over under a microscope. You will see mask defined pads.
Xilinx is the biggest purveyor of "do as I say, not as I do". In their guidelines, they insist, using the logic Vladimir puts forth, that non-mask defined pads are superior.
We usually work with small balls. The "weak link in the chain" with these is the adhesion of the pad to the laminate, not cracks in the solder. Kyocera did a pretty decent study on this a few years ago, and concluded that the most robust designs used mask defined pads.
The big problems with mask defined pads are mask contamination on the pads and poor solder mask resolution on behalf of most pcb fabricators. If the fab can do a good job on the mask, you will get stronger, more uniform as-reflowed balls.
Maybe the big parts work totally different from my small ones, but I have not seen any problems with mask defined pads other than those stated above.
Wayne Thayer
________________________________
From: TechNet on behalf of Igoshev, Vladimir
Sent: Tue 3/18/2008 9:18 AM
To: [log in to unmask]
Subject: Re: [TN] Solder Mask Defined Pad BGA Reliability
There is a very short answer: Fracture Mechanics :-)
When we have an SMD pad, there is an unavoidable stress concentration in
the vicinity of the triple junction "solder/solder pad/solder mask".
Non-SMD pads are free from that kind of stress concentration, as they
are "wrapped up" with solder.
Regards,
Vladimir
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kirk, Graham (GE
EntSol, Intelligent Platforms)
Sent: Tuesday, March 18, 2008 8:06 AM
To: [log in to unmask]
Subject: Re: [TN] Solder Mask Defined Pad BGA Reliability
Hi Joyce,
I realize that CTE mismatch is responsible for the fatigue, I am trying
to understand why the solder mask has so much effect on the solder
joint.
Graham Kirk
Senior Technologist
Radstone Embedded Computing
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
Sent: 18 March 2008 11:07
To: [log in to unmask]
Subject: Re: [TN] Solder Mask Defined Pad BGA Reliability
Fatique, due to CTE mismatch or poor design. My 1st guess.
Jk
--------------------------
Sent using BlackBerry
----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Tue Mar 18 06:18:08 2008
Subject: [TN] Solder Mask Defined Pad BGA Reliability
Hi All,
Can anybody tell me what the actual mechanism is that propagates cracks
in the device to ball joint on plastic BGA's (Leaded balls) with SMD
pads under thermal cycling?
Graham Kirk
Senior Technologist
GE Fanuc Intelligent Platforms Ltd
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute
non-public information. Any use of this information by anyone other than
the intended recipient is prohibited. If you have received this
transmission in error, please immediately reply to the sender and delete
this information from your system. Use, dissemination, distribution, or
reproduction of this transmission by unintended recipients is not
authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|