Of course with that approach you probably wouldn't have a prayer - you
could of course to negotiate a transfer contract to the Vatican Cardinals of
Fitzgerald in which case they would welcome you with open alms
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey (EHCOE)
Sent: Monday, March 03, 2008 10:14 AM
To: [log in to unmask]
Subject: Re: [TN] Gold Plating Question
I knew you wood worm your way into this conversation. I am always
appreciative of anyone who acknowledges my humor. It keeps me in good
spirits.
Yes, I did. I even got the rare chance to have an audience with the
Pope. If they asked what religious association I was representing, I was
going to reply the Arizona Cardinals; hoping that was enough penitence
to get in.
Dewey
-----Original Message-----
From: John Burke [mailto:[log in to unmask]]
Sent: Monday, March 03, 2008 10:29 AM
To: 'TechNet E-Mail Forum'; Whittaker, Dewey (EHCOE)
Subject: RE: [TN] Gold Plating Question
Absinth does indeed make the heart grow fonder - good to have you back.
I trust that when in Rome you were Deweying as the Romans do?
John....8-)
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey
(EHCOE)
Sent: Monday, March 03, 2008 7:48 AM
To: [log in to unmask]
Subject: Re: [TN] Gold Plating Question
Well I was in Rome last week and it is refreshing to see that all of you
were able to maintain the highly technical and refined ambiance of this
forum in my absinths.
In one of the introductory courses of Dewey 101 is word history and
rules for use. I am aware of the term but have spelled it cafoufle(
spell check says kafuffle or caboodle). This makes it a colloquial
idiom, which is fine for local and/or colorful speech and Deweyisms;
however to be an acceptable technical word we will need to establish a
correct spelling and definition.
I will gladly champion (no syntax without representation) it's inclusion
in IPC-T-50 when that is accomplished.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas O. Pauls
Sent: Friday, February 29, 2008 8:38 AM
To: [log in to unmask]
Subject: Re: [TN] Gold Plating Question
Kerfuffle? I like it.
Dewey, lets add that to the IPC T-50 document.
Doug Pauls
Craig Cullum <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
02/29/2008 09:35 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Craig Cullum <[log in to unmask]>
To
[log in to unmask]
cc
Subject
Re: [TN] Gold Plating Question
I just wanted to let everyone who participated in this thread that I
very
much appreciated learning something new. We recently experienced this
for
the first time (that I ever recall) and it caused a small kerfuffle and
some embarrassement on my part.
Thank you (from one lurker) !
Craig Cullum, Engineering Technologist, AMTELCO
e: [log in to unmask]
[log in to unmask]
f: 608 838 8367
v: 608 838 4194, or 4197, x128
Please visit us at www.amtelco.com
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Greene
> Sent: Wednesday, February 27, 2008 3:07 PM
> To: [log in to unmask]
> Subject: Re: [TN] Gold Plating Question
>
<SNIP>
> Depending on the chamfer, the design itself may result in a
> piece of the buss bars being left. In either case, exposed
> copper will be seen and is acceptable per IPC-A-600.
> Paul Greene
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|