Karl,
Could you tool up a disposable vinyl "Cap-plug", or would it not
withstand the cure temp? Ditto Steve's question of what thou art using,
and what it likes to cure at.
Ever tried Teflon, delrin, or UHMW as a mold? - a two-piece clamshell
affair.
With the exception of the Teflon, just give the two mold halves a quick
spray of carnuba wax mold release and 'knock yourself out'.
If you are not going for cosmetics, acrylic backed Kapton tape makes a
handy dandy mold at times too! - depending on your dexterity and
handiness :-)
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Karl Hunsinger
Sent: Wednesday, March 05, 2008 7:08 AM
To: [log in to unmask]
Subject: [TN] Unique potting requirements
Hi all,
I've asked Steve to post a few pictures of some unique potting
requirements. We currently make rubber potting molds, FR4 potting molds
and sometimes machined steel is used, however costly. The shape of this
potting doesn't lend itself to the mentioned methods of production. Any
ideas on how to achieve this shape would be greatly appreciated.
Sincerely,
Karl Hunsinger
Project Engineering
Flexible Circuits Inc.
215-343-2300 X5154
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
THE INFORMATION CONTAINED IN THIS E-MAIL MESSAGE AND ANY ATTACHMENTS SENT FROM GENTEX CORPORATION IS GENTEX CONFIDENTIAL INFORMATION INTENDED ONLY FOR THE PERSONAL USE OF THE INDIVIDUAL OR ENTITY NAMED ABOVE. If you are not the intended recipient, you are hereby notified that any review, distribution, or copying of this communication is strictly prohibited. If you have received this communication in error, please immediately notify the sender by return e-mail, and delete this e-mail message and any attachments from your computer.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|