TECHNET Archives

March 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Hfjord <[log in to unmask]>
Date:
Thu, 20 Mar 2008 19:43:14 +0100
Content-Type:
text/plain
Parts/Attachments:
text/plain (179 lines)
Xilinx made a number of analysis for me, superBGA solder joints on ENIG.
Normal NiSn was 0.7-1.0 um, but in some cases as much as 3.4 um. I'll send
the report to you off line.
/Inge




-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Wenger, George M.
Skickat: den 19 mars 2008 22:43
Till: [log in to unmask]
Ämne: Re: [TN] Case of the popping BGAs

1 micron  (40 microinches)  of NiSn IMC is hard to believe.  That is
much thicker than any NiSn IMC I've ever seen 

 

Regards,

George

George M. Wenger

Andrew Wireless Solutions

Senior Principal FMA / Reliability Engineer

40 Technology Drive, Warren, NJ 07059

(908) 546-4531 [Office]  (732) 309-8964 [Cell]

[log in to unmask]

 

________________________________

From: Igoshev, Vladimir [mailto:[log in to unmask]] 
Sent: Wednesday, March 19, 2008 5:35 PM
To: [log in to unmask]; Wenger, George M.
Subject: Re: [TN] Case of the popping BGAs

 

That well could be. The penetration depth is only around 1 micron.

Regards,

Vladimir

----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Wed Mar 19 17:30:54 2008
Subject: Re: [TN] Case of the popping BGAs




I have a hard time believing that at 10kV
Werner,



I have a hard time believing that at 10kV acceleration potential that
they see only the SnNi IMC and very little of the SnPb solder behind the
IMC.



Regards,

George

George M. Wenger

Andrew Wireless Solutions

Senior Principal FMA / Reliability Engineer

40 Technology Drive, Warren, NJ 07059

(908) 546-4531 [Office]  (732) 309-8964 [Cell]

[log in to unmask]



________________________________

From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Wednesday, March 19, 2008 5:15 PM
To: Wenger, George M.; [log in to unmask]
Subject: Re: [TN] Case of the popping BGAs



Hi George,
From my experience, what they seeing on the ball side is pretty much
SnNi IMC. What i find missing is any Au.



Werner



**************
Create a Home Theater Like the Pros. Watch the video on AOL Home.
(http://home.aol.com/diy/home-improvement-eric-stromer?video=15?ncid=aol
hom00030000000001)

------------------------------------------------------------------------
------------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information. 
If you have received it in error, please notify the sender
immediately and delete the original.  Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------
------------------------
[mf2]


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

----------------------------------------------------------------------------
--------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.  
If you have received it in error, please notify the sender
immediately and delete the original.  Any unauthorized use of
this email is prohibited.
----------------------------------------------------------------------------
--------------------
[mf2]


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2