Russ
Good point.
I recall in several of meetings on issues other than soldering, but
concerning PCBs that we were told that all of your processing folks always
had clean hands so that there would never be a transfer issue resulting from
handling at your facility. I remember this being expressed emphatically to
Richmond's senior management over a testing issue when they suggested your
shop should wear gloves to protect test points. It is good to know that "you
all" successfully resolved all of the issues mentioned below without going
to gloves.
Best regards
Lee
J. Lee Parker, Ph.D.
JLP Consultants LLC
804 779 3389
----- Original Message -----
From: "Nowland, Russell Howard (Russell)" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, February 28, 2008 3:36 PM
Subject: Re: [TN] OSP - protection
George,
There are a few items that you missed and one was the heavy southern
draaawl.
The other is you don't need gloves but it is advisable to only hand the
boards from the card edges.
There are still some bad elements that can transfer to the board and can
cause some soldering difficulties. Most of the issues we found were
hand lotions and pop corn oil.
So no selling pop corn in the vending machines and no Avon or Mary Kay
parties in the cafeteria and you don't need gloves.
Russell Nowland
Alcatel-Lucent
Advanced Manufacturing Engineer
Address: 14000 Quail Spring Parkway, Suite 300
Oklahoma City, OK 73134
email: [log in to unmask]
Desk: 405-302-1660
Cell: 405-203-0034
Fax: 405-302-1622
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wenger, George M.
Sent: Thursday, February 28, 2008 2:27 PM
To: [log in to unmask]
Subject: Re: [TN] OSP - protection
You should point out that none of your customers found glov
Lee,
You should point out that none of your customers found gloves necessary
with either OSP or immersion silver.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lee parker
Sent: Thursday, February 28, 2008 3:01 PM
To: [log in to unmask]
Subject: Re: [TN] OSP - protection
Genny
We had over 20 years of experience at the AT&T facility in Richmond with
OSPs. Our customers stored the boards side by side with HASL boards and
experienced no adverse effects. I will also point out that while gloves
give added protection, none of our customers found them necessary.
Best regards
Lee
J. Lee Parker, Ph.D.
JLP Consultants LLC
804 779 3389
----- Original Message -----
From: "Genny Gibbard" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, February 28, 2008 12:28 PM
Subject: [TN] OSP - protection
For immersion silver, we wear gloves when handling them prior to reflow,
and we interleave the silver saver paper and seal them in MBBs to store
them.
We are starting to work with OSP for the first time. What do you
recommend for OSP handling? Gloves is a given, but I am wondering about
storage.
Thanks in advance,
Genny.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
------------------------------------------------------------------------
------------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.
If you have received it in error, please notify the sender
immediately and delete the original. Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------
------------------------
[mf2]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|