Which newer ones? Can you name a few.
Victor,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of George Milad
Sent: Thursday, February 28, 2008 1:36 PM
To: [log in to unmask]
Subject: Re: [TN] OSP - protection
OSP finishes and specially the newer high temperature ones are more
robust
than the immersion silver as far as interaction with sulphur bearing
environment.
Standard packaging will keep OSP protection for the intended shelf
life.
Most of OSP deterioration occurs with thermal excursions during the
assembly
process.
Regards
George Milad
George Milad
National Accounts Manager for Technology
Uyemura International Corp (UIC)
249 Town Line Rd
Southington CT 06489
[log in to unmask]
Cell: (516) 901 3874
**************Ideas to please picky eaters. Watch video on AOL Living.
(http://living.aol.com/video/how-to-please-your-picky-eater/rachel-campo
s-duffy/
2050827?NCID=aolcmp00300000002598)
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------