Hi Graham - Sir Doug is at the Rockwell Collins Richardson TX facility for
a couple days but he typically checks his email in the evening so you will
see a reply later tonight. Apparently the daily high temperature of 0F
(excluding wind chill) scared him South where the Diet Mt. Dew won't
freeze. My recommendation is to use Ion Chromatography to demonstrate that
the components are "dirty". As Bev described, IC is soooo much better in
terms of definitive results.
Dave Hillman
Rockwell Collins
[log in to unmask]
Graham Collins <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
02/19/2008 11:35 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]
To
[log in to unmask]
cc
Subject
[TN] cleanliness testing
Hello TechNet
I'm in a debate with a supplier about the incoming cleanliness of one of
their parts, they claim it's squeaky clean and I claim it's as salty as a
bag of salt & vinegar potato chips. Obviously we are both exaggerating,
but one of us has a good claim.
They are fending me off with resistivity measurements made per the manual
test method IPC-TM-650 2.3.25 - which works in that I don't know how to
convert it to the "ug NaCl/in2" equivalent units I'm used to. Is there a
valid conversion?
Sir Doug of Dew, if you reply please do NOT say it depends...
regards,
Graham Collins
Halifax Production Engineering
L-3 communications Electronic Systems
(902) 873-2000 ext. 6215
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|