Dear Phil:
1. Have you done a dye and pry and confirmed that is indead the ball/board interface?
2. Have you completed an analysis of the pad to determine what if any constitutes are o the pads?
3. Are the cracks or opens across all areas of the BGA or just corners or one area?
Bob Wettermann
BEST
Phillip Bavaro <[log in to unmask]> wrote: I am wondering if anyone else out there has run into a problem with a
Samsung Flash memory device (in this case, the 0.8 mm pitch, 107 pin sac305
BGA) where the connections are cracking right at the interface between the
pwb and ball.
I had read about some Samsung BGA problems but cannot find the link to the
information now.
We have other BGA's on the same board without any issues. Shear strength
test results are very low as well (if the flash has not already popped off
by itself).
I'll try to get some pictures to Steve to put up tonight. My current
thoughts are CTE's are grossly mis-matched as we haven't found anything on
the pads to account for the gross failure.
Thanks in advance,
Phil
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
Bob Wettermann
PH 847-767-5745
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|