TECHNET Archives

February 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Ian Hanna <[log in to unmask]>
Date:
Fri, 29 Feb 2008 11:04:00 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Pasquito, Helena" <[log in to unmask]>
Subject:
From:
"Pasquito, Helena" <[log in to unmask]>
Content-Transfer-Encoding:
base64
In-Reply-To:
Content-Type:
text/plain; charset="UTF-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (1 lines)
Hello All,

Thank you for your responses regarding "gold fingers" and plating.  Seems that everyone involved in designing boards over the last half century or so has "tribal knowledge" of what is required but hunting it down in a specific specification was quite the challenge.  Fixing our requirements to our suppliers today.



My new word - kerfuffle!  Here's the googled definition and story.  



KERFUFFLE/kəˈfʌf(ə)l/ 

A commotion or fuss.



You will most commonly come across this wonderfully expressive word in Britain and the British Commonwealth countries (though the White House spokesman Ari Fleischer used it in January this year). It is rather informal, though it often appears in newspapers. One of the odder things about it is that it changed its first letter in quite recent times. Up to the 1960s, it was written in all sorts of ways — curfuffle, carfuffle, cafuffle, cafoufle, even gefuffle (a clear indication that its main means of transmission was in speech, being too rarely written down to have established a standard spelling). But in that decade it suddenly became much more popular and settled on the current kerfuffle. Lexicographers suspect the change came in response to the way that a number of imitative words were spelled, like kerplop and kerplunk.



In those cases, the initial ker– adds emphasis, as it does in other words, perhaps onomatopoeic but perhaps also borrowing the first syllable of crash. But we know kerfuffle was originally Scots and it’s thought that its first part came from Scots Gaelic car, to twist or bend. The second bit is more of a puzzle: there is a Scots verb fuffle (now known only in local dialect), to throw into disorder, dishevel, or ruffle. No obvious origin for it is known and experts suspect it was an imitative word. It is probably linked with Scots fuff, to emit puffs of smoke or steam, definitely imitative, which in the late eighteenth century also had a sense of going off in a huff or flying into a temper.



Some specialists think kerfuffle is also related to the Irish cior thual, confusion or disorder. It seems to be a minority opinion, though.



World Wide Words is copyright © Michael Quinion, 1996–2008. All rights reserved. Contact the author if you want to reproduce this piece, but first see our advice page, which also has notes about linking. Your comments and corrections are welcome. Page created 18 May 2002.

Helena Pasquito

Manufacturing Skills Instructor

Tyco Electronics, Wireless Systems Segment

1011 Pawtucket Blvd., M/S 107

Lowell, MA 01853

978-442-5024

[log in to unmask]





-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Ian Hanna

Sent: Friday, February 29, 2008 10:55 AM

To: [log in to unmask]

Subject: Re: [TN] Gold Plating Question



Best to define acceptable limits for kerfuffle for Class I/II/III



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas O. Pauls

Sent: Friday, February 29, 2008 10:38 AM

To: [log in to unmask]

Subject: Re: [TN] Gold Plating Question



Kerfuffle?  I like it.



Dewey, lets add that to the IPC T-50 document.



Doug Pauls









Craig Cullum <[log in to unmask]> 

Sent by: TechNet <[log in to unmask]>

02/29/2008 09:35 AM

Please respond to

TechNet E-Mail Forum <[log in to unmask]>; Please respond to

Craig Cullum <[log in to unmask]>





To

[log in to unmask]

cc



Subject

Re: [TN] Gold Plating Question













I just wanted to let everyone who participated in this thread that I

very

much appreciated learning something new. We recently experienced this

for

the first time (that I ever recall) and it caused a small kerfuffle and

some embarrassement on my part.



Thank you (from one lurker) !



Craig Cullum, Engineering Technologist, AMTELCO

e: [log in to unmask]

   [log in to unmask]

f: 608 838 8367

v: 608 838 4194, or 4197, x128



Please visit us at www.amtelco.com 



> -----Original Message-----

> From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Greene

> Sent: Wednesday, February 27, 2008 3:07 PM

> To: [log in to unmask]

> Subject: Re: [TN] Gold Plating Question

> 

<SNIP>

> Depending on the chamfer, the design itself may result in a 

> piece of the buss bars being left. In either case, exposed 

> copper will be seen and is acceptable per IPC-A-600.

> Paul Greene



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text

in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to 

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to 

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 

for additional information, or contact Keach Sasamori at [log in to unmask]

or 

847-615-7100 ext.2815

-----------------------------------------------------





---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text

in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------


ATOM RSS1 RSS2